46 C.F.R. § 56.80-5   Bending.


Title 46 - Shipping


Title 46: Shipping
PART 56—PIPING SYSTEMS AND APPURTENANCES
Subpart 56.80—Bending and Forming

Browse Next

§ 56.80-5   Bending.

Pipe may be bent by any hot or cold method and to any radius which will result in a bend surface free of cracks, as determined by a method of inspection specified in the design, and substantially free of buckles. Such bends shall meet the design requirements of 102.4.5 and 104.2.1 of ANSI-B31.1. This shall not prohibit the use of bends designed as creased or corrugated. If doubt exists as to the wall thickness being adequate, Class I piping having diameters exceeding 4 inches shall be nondestructively examined by the use of ultrasonics or other acceptable method. Alternatively, the pipe may be drilled, gaged, and fitted with a screwed plug extending outside the pipe covering. The nondestructive method shall be employed where the design temperature exceeds 750 °F. Prior to the use of nondestructive method of examination by the above procedure, it shall be demonstrated by the user, in the presence of a marine inspector on specimens similar to those to be examined, that consistent results, having an accuracy of plus or minus 3 percent, can be obtained.

[CGFR 68–82, 33 FR 18843, Dec. 18, 1968, as amended by CGFR 69–127, 35 FR 9979, June 17, 1970]

Browse Next

chanrobles.com


ChanRobles Legal Resources:

ChanRobles On-Line Bar Review

ChanRobles Internet Bar Review : www.chanroblesbar.com

ChanRobles MCLE On-line

ChanRobles Lawnet Inc. - ChanRobles MCLE On-line : www.chanroblesmcleonline.com